MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ASTM A516, Grade 55
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel; Nonresulfurized Steel; Pressure Vessel Steel

Material Notes: Carbon steel plate for moderate and lower temperature service. Maximum plate thickness is only limited by the capacity of the composition to meet the specified mechanical property requirements; however, current production of ASTM A516 Grade 55 plates are normally limited to maximum thickness of 12 in. (305 mm).

Key Words: SA516
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 380 - 515 MPa
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.26 %
Iron, Fe 98 %as balance
Manganese, Mn 0.60 - 1.2 %may vary with plate thickness
Phosphorus, P 0.035 %
Silicon, Si 0.15 - 0.40 %
Sulfur, S 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A516, Grade 60
ASTM A516 Carbon Steel, Grade 70
ASTM A516 Carbon Steel, Grade 65
ASTM A285, Grade A
ASTM A285, Grade C

MASTMA516A / 10277

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.