MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Jilin Xingyun Chemical T613 Viscosity index improver
Categories: Other Engineering Material

Material Notes: The product is mainly applied in improving and increasing lube oil viscosity. It has a good compatibility with other additives, and it will have no side effect on other index.
(1) Thickening ability: The thickening ability of Ethylene-propylene copolymer viscosity index improver varies with the brands. T-612 has a better thickening ability than other brands
(2) Shearing stability: The performance of shearing stability varies with the volume of molecular weight and its distribution of width. T-614 is superior to T-612?T-613.
(3) Thermal oxidation stability: The product of ethylene-propylene copolymer viscosity index improver shows an excellent thermal oxidation stability with heat-resistance and no decomposition under high temperature conditions.
(4) Low temperature performance: T-614 shows a good performance under low temperature. There is little influence to the low temperature pumping performance of multi-grade lube oils by the single application of T-614, which is better than other brands of additives.
(5) T-612A?T-613A?T-614A are all high-viscosity products which have particular excellent thickening ability; T-615A is also a high-viscosity product, which has better ability in thickening and shearing stability.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 - 0.880 g/cc0.0311 - 0.0318 lb/in³
Kinematic Viscosity 850 cSt
@Temperature 100 °C
850 cSt
@Temperature 212 °F
dynamic
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 170 °C>= 338 °Fopen
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %
 
Descriptive Properties
AppearanceYellowish or yellow transparent sticky liquid
Color<2Chroma
Content<0.08%Mechanical Impurities
Dispersity SDT>60
Shearing stability<35by diesel oil nozzle (100?), Shearing stability index: SSI
Thickening Ability>0.5 mm2/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJILINX041 / 317888

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.