MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TBA ECP 592/CAN Permanently Conductive Graphene Hybrid Clear Acrylic Coating Aerosol
Categories: Other Engineering Material

Material Notes: Single component permanently conductive graphene hybrid clear acrylic coating which provides effective static elimination for electronics safe handling area and explosive atmosphere applications. Fully compliant with BS EN 61340-5-1:2007 and ATEX. Contains carbon nanotubes and graphene derivative. Applications in lighting , windows, clear covers and lids, displays etc. Supplied as an aerosol for ease of application.

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1.00e+7 ohm
@Thickness 0.0500 mm
<= 1.00e+7 ohm
@Thickness 0.00197 in
ASTM D257
Static Decay <= 2.0 sec<= 2.0 secIEC TC15
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 87 %87 %
 
Processing PropertiesMetricEnglishComments
Cure Time 720 min12.0 hourfull

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTBA037 / 281515

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.