MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro MULTRANOL® 8164 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Multranol 8164 is a sucrose-based polyether polyol.

Properties / Applications: Multranol 8164 is a sucrose-based polyether polyol used in the manufacture of rigid polyurethane foams. Multranol 8164 is an excellent general purpose polyol which shows good compatibility with a wide range of foam ingredients including other polyether and polyester polyols, catalysts, surfactants and various blowing agents. As with any product, use of Multranol 8164 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity  1.10 g/cc
@Temperature 25.0 °C
1.10 g/cc
@Temperature 77.0 °F
 1.105 g/cc
@Temperature 51.0 °C
1.105 g/cc
@Temperature 124 °F
 1.11 g/cc
@Temperature 40.0 °C
1.11 g/cc
@Temperature 104 °F
Bulk Density 1.09 g/cc0.0394 lb/in³
Viscosity  2500 cP
@Temperature 40.0 °C
2500 cP
@Temperature 104 °F
 5000 cP
@Temperature 30.0 °C
5000 cP
@Temperature 86.0 °F
 >= 10500 cP
@Temperature 25.0 °C
>= 10500 cP
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 200 °C>= 392 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.17 %<= 0.17 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0936 / 202719

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.