MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron™ NSM PA6 Nylon, Cast Solid Lubricant Filled, Type 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber/Solid Lube Filled

Material Notes: The most wear-resistant nylon available, this self-lubricating cast nylon has a dynamic load-bearing capacity up to five times higher and a service life up to 10 times longer than conventional cast nylons.

Key Words: Polyamide 6; PA6; PA 6
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Water Absorption at Saturation 7.00 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 81.0ASTM D785
Hardness, Shore D 76.0ISO 868
Tensile Strength 80.0 MPaISO 527-1/-2 (7)
Elongation at Yield 5.00 %ISO 527-1/-2 (7)
Flexural Strength 109 MPaISO 178 (12)
Compressive Yield Strength 31.0 MPa
@Strain 1.00 %
ISO 604 (10)
 59.0 MPa
@Strain 2.00 %
ISO 604 (10)
 87.0 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 69.0 MPaASTM D732
Charpy Impact, Notched 3.50 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Strength 25.0 kV/mmIEC 60243-1 (15)
 400 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µin/in-°FASTM E-831 (TMA)
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 95.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.290 W/m-K
Melting Point 420 °FASTM D3418
Maximum Service Temperature, Air 200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 200 °FASTM D648
Minimum Service Temperature, Air -30.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ GSM PA6 Nylon, Cast MoS2 Filled Type 6
Mitsubishi Chemical Advanced Materials Nylatron™ GSM Blue PA6 Cast Oil & MoS2 Filled Type 6
Mitsubishi Chemical Advanced Materials Nylatron™ MC 901 H.S. PA6
Mitsubishi Chemical Advanced Materials Nylatron™ MC™ 907 / Ertalon™ 6 PLA PA6 Unfilled Type 6 nylon
Mitsubishi Chemical Advanced Materials Nylatron™ 703 XL PA6 Cast, Wear Resistant, Zero 'Stick-Slip

P1SM25 / 20113

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.