MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Green Dot Terratek® NF3010 (Preliminary) Polypropylene, 30% Natural Fiber Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Terratek® NF3010 is a proprietary blend of natural fiber and reprocessed polypropylene for injection molding applications. NF3010 contains 30% natural fiber by weight.

Information provided by Green Dot Bioplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D792
Melt Flow 2.77 g/10 min
@Load 2.06 kg,
Temperature 190 °C
2.77 g/10 min
@Load 4.54 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 38.5 MPa5580 psiASTM D638
Elongation at Break 4.8 %4.8 %
Tensile Modulus 2.48 GPa360 ksiASTM D638
Izod Impact, Notched 1.01 J/cm1.90 ft-lb/inASTM D256
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 182 °C350 - 360 °F
Middle Barrel Temperature 177 - 182 °C350 - 360 °F
Front Barrel Temperature 182 - 191 °C360 - 375 °F
Nozzle Temperature 182 - 191 °C360 - 375 °F
Melt Temperature <= 204 °C<= 400 °F
Mold Temperature 15.6 - 76.7 °C60.0 - 170 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGREEND5029 / 312300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.