Physical Properties | Original Value | Comments |
---|
Density | 1.0574 g/cc @Temperature 100 °C |
| 1.0668 g/cc @Temperature 100 °C |
| 1.0761 g/cc @Temperature 100 °C |
| 1.0853 g/cc @Temperature 100 °C |
| 1.0942 g/cc @Temperature 100 °C |
| 1.0986 g/cc @Temperature 40.0 °C |
| 1.1085 g/cc @Temperature 40.0 °C |
| 1.1087 g/cc @Temperature -5.00 °C |
| 1.1183 g/cc @Temperature 40.0 °C |
| 1.12 g/cc @Temperature -5.00 °C |
| 1.128 g/cc @Temperature 40.0 °C |
| 1.1314 g/cc @Temperature -5.00 °C |
| 1.1426 g/cc @Temperature -5.00 °C |
| 1.1537 g/cc @Temperature -5.00 °C |
| 1.888 g/cc @Temperature 40.0 °C |
Viscosity | 0.45 cP @Temperature 100 °C |
| 0.53 cP @Temperature 100 °C |
| 0.56 cP @Temperature 80.0 °C |
| 0.65 cP @Temperature 80.0 °C |
| 0.70 cP @Temperature 100 °C |
| 0.72 cP @Temperature 60.0 °C |
| 0.83 cP @Temperature 60.0 °C |
| 0.84 cP @Temperature 80.0 °C |
| 0.98 cP @Temperature 40.0 °C |
| 1.06 cP @Temperature 60.0 °C |
| 1.1 cP @Temperature 40.0 °C |
| 1.37 cP @Temperature 40.0 °C |
| 1.39 cP @Temperature 20.0 °C |
| 1.54 cP @Temperature 20.0 °C |
| 1.71 cP @Temperature 10.0 °C |
| 1.87 cP @Temperature 10.0 °C |
| 1.88 cP @Temperature 20.0 °C |
| 2.13 cP @Temperature 0.000 °C |
| 2.25 cP @Temperature 10.0 °C |
| 2.32 cP @Temperature 0.000 °C |
| 2.73 cP @Temperature -10.0 °C |
| 2.75 cP @Temperature 0.000 °C |
| 2.96 cP @Temperature -10.0 °C |
| 3.43 cP @Temperature -10.0 °C |
Molecular Weight | 36.47 g/mol |
Vapor Pressure | 0.00100 bar @Temperature -10.0 °C |
| 0.00200 bar @Temperature -10.0 °C |
| 0.00200 bar @Temperature -10.0 °C |
| 0.00300 bar @Temperature 0.000 °C |
| 0.00300 bar @Temperature 0.000 °C |
| 0.00300 bar @Temperature 0.000 °C |
| 0.00700 bar @Temperature 10.0 °C |
| 0.00700 bar @Temperature 10.0 °C |
| 0.00700 bar @Temperature 10.0 °C |
| 0.0130 bar @Temperature 20.0 °C |
| 0.0140 bar @Temperature 20.0 °C |
| 0.0150 bar @Temperature 20.0 °C |
| 0.0440 bar @Temperature 40.0 °C |
| 0.0460 bar @Temperature 40.0 °C |
| 0.0540 bar @Temperature 40.0 °C |
| 0.130 bar @Temperature 60.0 °C |
| 0.130 bar @Temperature 60.0 °C |
| 0.170 bar @Temperature 60.0 °C |
| 0.330 bar @Temperature 80.0 °C |
| 0.330 bar @Temperature 80.0 °C |
| 0.430 bar @Temperature 80.0 °C |
| 0.750 bar @Temperature 100 °C |
| 0.790 bar @Temperature 100 °C |
| 1.12 bar @Temperature 100 °C |
Surface Tension | 0.064 dynes/cm @Temperature 100 °C |
| 0.064 dynes/cm @Temperature 100 °C |
| 0.065 dynes/cm @Temperature 100 °C |
| 0.066 dynes/cm @Temperature 80.0 °C |
| 0.067 dynes/cm @Temperature 80.0 °C |
| 0.067 dynes/cm @Temperature 80.0 °C |
| 0.068 dynes/cm @Temperature 60.0 °C |
| 0.068 dynes/cm @Temperature 60.0 °C |
| 0.068 dynes/cm @Temperature 60.0 °C |
| 0.069 dynes/cm @Temperature 40.0 °C |
| 0.070 dynes/cm @Temperature 40.0 °C |
| 0.070 dynes/cm @Temperature 40.0 °C |
| 0.070 dynes/cm @Temperature 20.0 °C |
| 0.071 dynes/cm @Temperature 20.0 °C |
| 0.071 dynes/cm @Temperature 10.0 °C |
| 0.071 dynes/cm @Temperature 10.0 °C |
| 0.072 dynes/cm @Temperature 20.0 °C |
| 0.072 dynes/cm @Temperature 10.0 °C |
| 0.072 dynes/cm @Temperature -10.0 °C |
| 0.072 dynes/cm @Temperature -10.0 °C |
| 0.072 dynes/cm @Temperature 0.000 °C |
| 0.072 dynes/cm @Temperature 0.000 °C |
| 0.073 dynes/cm @Temperature 0.000 °C |
| 0.074 dynes/cm @Temperature -10.0 °C |
|
Thermal Properties | Original Value | Comments |
---|
Specific Heat Capacity | 2.40 J/g-°C @Temperature -10.0 °C |
| 2.50 J/g-°C @Temperature -10.0 °C |
| 2.50 J/g-°C @Temperature 0.000 °C |
| 2.60 J/g-°C @Temperature 0.000 °C |
| 2.60 J/g-°C @Temperature 10.0 °C |
| 2.60 J/g-°C @Temperature 20.0 °C |
| 2.70 J/g-°C @Temperature 20.0 °C |
| 2.70 J/g-°C @Temperature 40.0 °C |
| 2.70 J/g-°C @Temperature 10.0 °C |
| 2.80 J/g-°C @Temperature 60.0 °C |
| 2.80 J/g-°C @Temperature 40.0 °C |
| 2.80 J/g-°C @Temperature -10.0 °C |
| 2.80 J/g-°C @Temperature 0.000 °C |
| 2.90 J/g-°C @Temperature 10.0 °C |
| 2.90 J/g-°C @Temperature 60.0 °C |
| 2.90 J/g-°C @Temperature 20.0 °C |
| 3.00 J/g-°C @Temperature 40.0 °C |
| 3.00 J/g-°C @Temperature 80.0 °C |
| 3.10 J/g-°C @Temperature 100 °C |
| 3.10 J/g-°C @Temperature 80.0 °C |
| 3.10 J/g-°C @Temperature 60.0 °C |
| 3.20 J/g-°C @Temperature 80.0 °C |
| 3.20 J/g-°C @Temperature 100 °C |
| 3.30 J/g-°C @Temperature 100 °C |
Thermal Conductivity | 0.440 W/m-K @Temperature -10.0 °C |
| 0.450 W/m-K @Temperature -10.0 °C |
| 0.450 W/m-K @Temperature 0.000 °C |
| 0.460 W/m-K @Temperature 0.000 °C |
| 0.460 W/m-K @Temperature 10.0 °C |
| 0.470 W/m-K @Temperature 20.0 °C |
| 0.470 W/m-K @Temperature 10.0 °C |
| 0.480 W/m-K @Temperature 20.0 °C |
| 0.480 W/m-K @Temperature -10.0 °C |
| 0.490 W/m-K @Temperature 0.000 °C |
| 0.490 W/m-K @Temperature 40.0 °C |
| 0.500 W/m-K @Temperature 10.0 °C |
| 0.510 W/m-K @Temperature 60.0 °C |
| 0.510 W/m-K @Temperature 40.0 °C |
| 0.510 W/m-K @Temperature 20.0 °C |
| 0.520 W/m-K @Temperature 60.0 °C |
| 0.530 W/m-K @Temperature 40.0 °C |
| 0.530 W/m-K @Temperature 80.0 °C |
| 0.540 W/m-K @Temperature 80.0 °C |
| 0.550 W/m-K @Temperature 100 °C |
| 0.550 W/m-K @Temperature 60.0 °C |
| 0.560 W/m-K @Temperature 100 °C |
| 0.570 W/m-K @Temperature 80.0 °C |
| 0.590 W/m-K @Temperature 100 °C |
Melting Point | -85.0 °C |
| -66.0 °C |
| -60.0 °C |
| -59.0 °C |
Boiling Point | 98.0 °C @Pressure 0.101 MPa |
| 105 °C @Pressure 0.101 MPa |
| 109 °C @Pressure 0.101 MPa |
| 109 °C @Pressure 0.101 MPa |
|
Descriptive Properties |
---|
Composition | <2 mg/kg |
| <20 mg/kg |
| <3 mg/kg |
| <5 mg/kg |
| 300-320 g/kg |