MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nylon

(Viewing data as-entered. Click here to return)
Nylacast PA6C Cast Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Cast Nylons are a range of polyamides produced by a casting process involving the anionic polymerisation of caprolactam. This process allows the production of semi-finished plate, rod, tube and custom castings that are largely free of internal stresses. Nylacast PA 6 Natural (also available in black) is the basic PA 6 grade from which all the other grades of cast nylon stem. Generally accepted as the primary engineering polymer, natural cast nylon is suitable for virtually any plain bearing application, not to mention a huge range of other applications for which this versatile grade finds a use. By varying the conditions of polymerisation the mechanical properties of cast nylon may be altered to suit specific applications and the performance of the basic polymer can be enhanced with the addition of various additives, fillers, lubricants and colourants (see further grades). Compared with injection moulding and extrusion grades of polyamide, cast nylons stand out with their improved mechanical, thermal and chemical resistance properties. Specifically as the material has a higher tensile, compressive and impact strength as well as an improved resistance to creep and heat ageing. The reasons for these improved characteristics are high crystalinity and a remarkably higher molecular weight. Due to low water absorption, mechanical properties and dimensions are more stable, making it suited for components that have to meet closer tolerances. Abrasion resistance and overall wear performance are probably the material’s most important characteristics. For use in bearing applications and in applications where food contact is involved, cast nylons may be offered as a material conforming to FDA approvals. Natural cast nylon has the ability to operate effectively without the need for lubricants and has an increased resistance to wear of over 5 times that for plain bearings manufactured from non-ferrous metals. As is the case with virtually all nylons it is easy to machine, pleasant to work with and relatively light weight – one eighth that of brass – making the handling and fitting of large components manufactured in cast nylon a relatively easy matter

Benefits:

  • Good mechanical, thermal and chemical resistance properties
  • Universally acknowledged as the primary engineering polymer
  • Good PV and load bearing capabilities
  • Improved characteristics over extruded polymides
  • Good wear and abrasion resistance
  • Good dimensional stability, largely free from internal stresses
  • FDA Compliance
  • Available in a wide range of sizes and colours
Typical Application:
  • Rollers
  • Switch collar
  • Washers
  • Bearings
  • Load support
  • Bushes
  • Centralizers
  • Cable drums
  • Guide clutch
  • Seals
  • Blockers
  • Wear pads
  • Chain Guide
  • Clamps
  • Bespoke Components

Information provided by Nylacast Ltd.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccmethod A; ISO 1183:1987
Water Absorption 0.30 %
@Time 86400 sec
Immersion; ISO 62:1999
Moisture Absorption at Equilibrium 2.5 %50% RH, 23°C; ISO 62:1999
Water Absorption at Saturation 7.0 %Immersion; ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ISO 868:2003
Tensile Strength, Yield 75.0 - 80.0 MPaType 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3400 - 3600 MPaE-modulus; Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 105 - 125 MPa1.5mm/min; ISO 178:2001
Flexural Modulus 3300 - 3600 MPa1.5mm/min; ISO 178:2001
Compressive Strength 95.0 - 120 MPaType B, 5mm/min; ISO 604:2002
Compressive Modulus 2100 - 2700 MPaType B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 4.50 - 6.00 kJ/m²Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.16
@Pressure 1.75 MPa
31.4m/min
K Factor (Wear Factor) 430000[m*3/Nm], 31.4m/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mmIEC 60243-1:1998-01
Dissipation Factor 0.020
@Frequency 100 Hz
IEC 60250:1969-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Thermal Conductivity 0.260 W/m-KMean T=20°C; ISO 8301:1991
Melting Point 220 °C
Maximum Service Temperature, Air 170 °CIntermittent
 100 °C
@Time 1.80e+7 sec
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75
Minimum Service Temperature, Air -100 °CIntermittent
 -40.0 °CContinuous
Glass Transition Temp, Tg 65.0 °CISO 11359:1999
Flammability, UL94 HBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorNatural/Black/Other
Limiting PV100 MPa/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, Cast
PolyPLASTY PolyJARID PA 6 E Polyamide 6 extruded, Dry
Overview of materials for Nylon 66, Unreinforced
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized

PNYLAC01 / 89259

Nylon

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.