Bayblend® MTR AG sheet is a high performance product extension of Bayblend MTR sheet providing increased resistance to graffiti, scratches, cleaning chemicals, and foodstuff stains. This opaque flame retardant polycarbonate based sheet offers a unique combination of flammability characteristics, robust mechanical properties, and ease of fabrication. Bayblend MTR AG complies with the flammability and smoke emission requirements for transit materials per the U.S. Federal Railroad Administration, listed in DOT: 49 CFR 238, and meets the criteria in the Bombardier Transportation Standard SMP 800-C for Toxic Gas Generation. Bayblend MTR AG has a lower specific gravity, higher stiffness, higher strength, and greater toughness than typical non-metallic materials used for mass transportation interior components. This combination of physical properties allows for design of thinner and lighter parts that often do not require secondary reinforcement or stiffeners in the application. Bayblend MTR AG is available in a variety of textures and colors or custom printed decoration. Applications: Thermoformed rail interior parts, such as seating components, wall cladding, window reveals, and ceiling panels Information provided by Covestro |