MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Edinburg Plastics EGI608 Polyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Appearance: High Gloss Colors

Processing Methods: Injection

Applications: General Purpose

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792-91
Linear Mold Shrinkage, Flow 0.013 - 0.018 cm/cm
Linear Mold Shrinkage, Transverse 0.016 - 0.022 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8000 psiASTM D638
Elongation at Break 8.0 %ASTM D638
Flexural Yield Strength 12000 psiASTM D790
Flexural Modulus 340000 psiASTM D790
Izod Impact, Notched 0.750 ft-lb/inASTM D256
 
Processing PropertiesOriginal ValueComments
Feed Temperature 38.0 - 49.0 °C
Rear Barrel Temperature 249 - 260 °C
Middle Barrel Temperature 271 - 274 °C
Front Barrel Temperature 265 - 274 °C
Nozzle Temperature 260 - 271 °C
Melt Temperature 260 - 271 °C
Mold Temperature 27.0 - 57.0 °C
Drying Temperature 120 °C
Dry Time 4.00 - 24.0 hour
Moisture Content <= 0.020 %
Dew Point >= -40.0 °F
Back Pressure 50.0 - 120 psiLower is better
Screw Speed 40 - 70 rpmLower is better

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aegirine (Acmite), NaFe(SiO3)2

PEDIN060 / 183563

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.