MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aremco Crystalbond™ 509-2 Clear Turquoise Washaway Mounting Adhesive & Accessory
Categories: Polymer; Adhesive

Material Notes: Mid-range melting point of 165 ºF (74 ºC). Provides excellent adhesion and minimizes clogging of diamond tools when compared to many waxes. Transparent in thin cross-sections. Soluble in acetone or Aremco’s proprietary Crystalbond™ 509-S Stripper, a low odor, non-flammable, biodegradable, water-rinsible solvent. Available in three standard colors and both round sticks and rectangular bars.

Typical Applications

  • Machining advanced ceramics
  • Lapping and polishing optical components
  • Dicing ceramic substrates
  • Dicing semiconductor wafers
  • Dicing ferrites, glasses and piezoelectrics
  • Dicing metal and optical single crystals
  • Mounting cross-sections for SEM
  • Backfilling components for support
  • Dry plasma etching

Vendors: Aremco’s Crystalbond and Wafer-Mount products are ideal for temporarily mounting ceramics, glass, quartz, and semiconductor substrates for dicing and polishing operations. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity  1250 cP
@Temperature 127 °C
1250 cP
@Temperature 261 °F
#2 Spindle @ 12 rpm
 2500 cP
@Temperature 116 °C
2500 cP
@Temperature 241 °F
#2 Spindle @ 6 rpm
 5000 cP
@Temperature 102 °C
5000 cP
@Temperature 216 °F
#2 Spindle @ 3 rpm
 10000 cP
@Temperature 85.0 °C
10000 cP
@Temperature 185 °F
#2 Spindle @ 1.5 rpm
 25000 cP
@Temperature 74.0 °C
25000 cP
@Temperature 165 °F
#2 Spindle @ 1 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 8.00 MPa1160 psi
 
Thermal PropertiesMetricEnglishComments
Melting Point 74.0 °C165 °FFlow Point
 
Descriptive Properties
Available FormsRectangular Stick, 7/8” × 1” × 7”509-3B
 Round Stick, 5/8” Dia × 7”509-3A
Solvent509-S or Acetone
Weight0.20 Lbs/Stick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM31C / 316409

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.