Characteristics: High melt flow rate control reologhy Random copolymer polypropylene with very good optical properties and easy mold filling; fast cycle time; good impact resistance; with clarify and mold release additives. Recommended for: High clarity and good impact resistance injection molding storing boxes (big storage containers); thin walled injection molding package and general purpose applications where clarity is important. Information provided by Esenttia by Propilco |