MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gray Cast Iron, ASTM A 48 Class 40
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Carbon listed in the composition table is the total carbon. Can be oil quench hardened from 860°C to attain a Rockwell C 50 minimum surface hardness. Data provided by the manufacturer, Siltin Industries, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.15 g/ccTypical for Gray Cast Iron
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 183 - 234
Hardness, Knoop 258Converted from Brinell
Hardness, Rockwell B 97Converted from Brinell
Hardness, Rockwell C 20Converted from Brinell
Hardness, Vickers 246Converted from Brinell
Tensile Strength, Ultimate >= 276 MPa
Ultimate Compressive Strength >= 1034 MPa
Machinability 0.0 %Very good machinability. No numerical rating available.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.25 - 3.5 %
Chromium, Cr 0.050 - 0.45 %
Copper, Cu 0.15 - 0.40 %
Iron, Fe 91.9 - 94.2 %As Balance
Manganese, Mn 0.50 - 0.90 %
Molybdenum, Mo 0.050 - 0.10 %
Nickel, Ni 0.050 - 0.20 %
Phosphorus, P <= 0.12 %
Silicon, Si 1.8 - 2.3 %
Sulfur, S <= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Gray Cast Iron
Overview of materials for Cast Iron
ASTM class 30 Standard gray iron test bars, as cast
SAE J431 automotive gray cast iron, SAE grade G1800
ASTM class 20 Standard gray iron test bars, as cast

DSI001 / 3092

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.