MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® E47-S1 Nylon 12 Elastomer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Heat- and light-stabilized compound based on polyamide 12 elastomer for molding of sport shoe soles. VESTAMID® E47-S1 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer. VESTAMID® E47-S1 is especially developed for sport shoe soles. It has good impact strength at low temperatures. VESTAMID® E47-S1 is supplied as cylindrical pellets in moisture-proof packaging, ready for processing. The process temperatures should be within a range of 180°C – 220°C. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.5 MPa3990 psiISO 527
Elongation at Break 420 %420 %Nominal; ISO 527
 450 %450 %ISO 527
Tensile Modulus 0.132 GPa19.1 ksiISO 527
50% Modulus 12.5 MPa
@Strain 50 %
12.5 MPa
@Strain 50 %
ISO 527
 
Thermal PropertiesMetricEnglishComments
Melting Point 157 °C315 °FISO 11357-1/-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Evonik VESTAMID® E62-S1 Nylon 12 Elastomer
Evonik VESTAMID® Care ML21 Medical Grade Nylon 12
EMS-Grivory Grilamid® L 25 Z PA12-I
Arkema Pebax® 7433 SA 01 MED TPA

PEVONIK830 / 243039

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.