MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resin Technology Group TIGA 291-EX Grey Medium Viscosity Polyamide Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 1 to 1 by weight.

Tiga 291 EX Grey is a medium viscosity polyamide/ epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance are desired. This 1 to 1 ratio, two-part adhesive is easily mixed and cured at room temperature and develops tough, strong bonds to a wide variety of materials including metals, glass, ceramics and plastics. Fully cured Tiga 291 EX Grey bonds offer superior thermal shock resistance, mechanical, electrical and impact resistant properties and low permeability to gases and vapors. The cured material has good dimensional stability and resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis and many other chemicals.

Applications:

This system is recommended for low-stress, high impact/high peel strength bonding applications of dissimilar materials. Some proven applications are repairing strain gages, sealing seams on fiberglass components, repair of printed circuits, bonding stainless inserts inside potentiometers, bonding glass to aluminum, bonding of Pyrex, wire to Lucite, rubber hose to steel tubing, metal to fiberglass, repairing plastic laminates and sealing polyurethane foam.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccOf hardener
 1.34 g/ccOf resin
Viscosity Measurement 40000
@Temperature 25.0 °C
Of hardener, RVT #7 @ 10 rpm
 50000
@Temperature 25.0 °C
Mixed
 60000
@Temperature 25.0 °C
Of resin, RVT #7 @ 10 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 110 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 48.0 hour
@Temperature 25.0 °C
Pot Life 100 min
@Temperature 25.0 °C
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Diamond, Natural
Taiwan Sheen Soon Sheenthane® AH-783 TPU for Hotmelt Adhesive
Malleable iron casting, Class 35018
M Chemical GUARD DOG™ UV770 HALS Light Stabilizer
Hong Kun Group UV 360 UV Absorber

PRESINT631 / 65515

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.