MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röhm PLEXIGLAS® Satinice df22 zk30 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: PLEXIGLAS® Satinice df22 zk 30 is an amorphous, impact-modified thermoplastic molding compound.

Typical properties of impact modified PLEXIGLAS® molding compound are:

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • the pleasant feel and sound of the moldings.
PLEXIGLAS® Satinice df22 zk30 is characterized by the following special properties:
  • good light diffusion combined with excellent light transmission
  • matte surfaces can be obtained by varying the extrusion parameters
  • good break resistance and impact strength
  • improved resistance to stress cracking
  • balanced property profile
Application: PLEXIGLAS® Satinice df22 zk 30 is used for injection molding as well as for extruding and coextruding panels and profiles.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccISO 1183
Melt Flow 1.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psi50 mm/min; ISO 527
Elongation at Break 23 %23 %Nominal; ISO 527
Elongation at Yield 4.3 %4.3 %50 mm/min; ISO 527
Tensile Modulus 2.20 GPa319 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 3.30 J/cm²15.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.310 J/cm²1.48 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 96.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
53.3 µin/in-°F
@Temperature 32.0 - 122 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FISO 75
Vicat Softening Point 102 °C216 °FB / 50; ISO 306
Glass Transition Temp, Tg 112 °C234 °FISO 11357
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 86 %86 %ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °FInjection Molding
Drying Temperature <= 85.0 °C<= 185 °FPredrying
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourPredrying, Desiccant-Type Drier
 
Descriptive Properties
Half-Value Angle11°DIN 5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9357 / 319974

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.