MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® NRG 2901 BK Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® NRG 2901 BK is a high viscosity, heat stabilized compound with exceptional mold release properties. Additionally VESTAMID® NRG 2901 BK is nucleated to reduce the cycle time and shrinkage of molded parts. Generally mechanical properties of compounds based on PA 12 vary little with changing humidity due to their low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, high abrasion resistance, low friction and good chemical resistance. The manufacturer recommends a processing temperature between 230°C and 260°C - in some cases up to 280°C - during the injection molding process. The mold temperature should be within a range of 60°C to 100°C. Drying at 80°C for 2 hours to 4 hours before processing is recommended. Polyamide 12 is a high performance thermo-plastic polymer with increased performance characteristics that translates into safe operations over the life of the installed pipe- line. It has a considerable record of safe and proven experience in many demanding applications, including fuel lines in passenger cars, air brake tubing in trucks and off-shore applications. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Energy, Oil and Gas
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering, Oil / fuels
Additives: Unfilled
Applications: Tube and hose
Processing: Pipe/Tube extrusion
Special Characteristics: Semi-crystalline, High heat resistant, High viscosity
Features: Low coefficient of friction
Color: Black
Additives: Heat stabilizer
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Moisture Absorption 0.700 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00700 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cmISO 294-4, 2577
Melt Flow 36.0 g/10 min
@Load 10.0 kg,
Temperature 235 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 76.0 MPaISO 2039-1
Tensile Strength at Break 53.0 MPaISO 527
Tensile Strength 45.0 MPaISO 527
Tensile Stress 36.0 MPa
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 45.0 MPaISO 527
Elongation at Break 225 %Nominal; ISO 527
Elongation at Yield 5.00 %ISO 527
Tensile Modulus 1560 MPaISO 527
Flexural Strength 40.0 MPaISO 178
Flexural Modulus 1300 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 177 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Vicat Softening Point 150 °C
@Load 5.10 kg
50 K/h; ISO 306
 175 °C
@Load 1.02 kg
50 K/h; ISO 306
Glass Transition Temp, Tg 40.0 °CISO 11357-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 294
 80.0 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption26.1 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.7 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.8 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7935 / 325067

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.