MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese N-325 Nylon 6/6  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Film

Material Notes: Description: Nylon N-325 is an intermediate viscosity nylon 6/6 that can be used for monofilament or extrusion applications (films).

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183 & ASTM D792
Moisture Absorption at Equilibrium 2.5 %at 50% RH; ISO 62
Water Absorption at Saturation 8.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ISO 2039-2
Tensile Strength at Break 12000 psiASTM D638
Tensile Strength, Yield 83.0 MPa50 mm/min; ISO 527-2/1A
Elongation at Break 45 %50 mm/min; ISO 527-2/1A
 40 - 80 %ASTM D638
Elongation at Yield 5.0 %50 mm/min; ISO 527-2/1A
Tensile Modulus 3.00 GPa1 mm/min; ISO 527-2/1A
Flexural Strength 17000 psiASTM D790
Flexural Modulus 2.80 GPaISO 178
 420000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.40 kJ/m²ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 257 °CASTM D3418
 263 °CISO 11357-1,2,3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 277 - 310 °C
Drying Temperature 140 °F
Dry Time 1 - 2 hour
Back Pressure 0.000 - 50.0 psi
Screw Speed 40 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese N-276 Glass/Mineral Reinforced Nylon 6/6
Celanese Hostaform® LX90Z XAP² ™ POM, UV Resistant
Celanese Celcon® TX90 Acetal Copolymer
Celanese 6423 Nylon 6/6, 14% Glass-Fiber Reinforced, Dry As Molded
Celanese 6423 Nylon 6/6, 14% Glass-Fiber Reinforced, at 50% RH

PHCV59 / 45900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.