MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Park Aerospace Nelco® N4000-7 EF® Halogen-Free Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free assembly designs.

Key Features and Benefits:

  • Outstanding moisture resistance and thermal stability
  • Uncompromised electrical values
  • Halogen-Free
  • CAF resistant
  • High Tg FR-4 processing

Applications/Qualifications:

  • Lead-Free Assemblies
  • Fine-Line Multilayers
  • Backplanes
  • Surface-Mount Multilayers
  • BGA Multilayers
  • Automotive Electronics
  • MCM-Ls
  • Direct Chip Attach
  • Wireless Communications
  • Telecommunications Infrastructure
  • RoHS Compliant
  • Meets IPC-4101/94 Specifications

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.92 g/cc0.0694 lb/in³50% Resin Content; Internal Method
Water Absorption 0.10 %0.10 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.982 kN/m5.60 pliafter exposure to process solutions; IPC-TM-650.2.4.8
 0.999 kN/m5.70 pliat elevated temperature; IPC-TM-650.2.4.8.2a
 1.17 kN/m6.70 pliafter solder float; IPC-TM-650.2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmC - 96/35/90; IPC-TM-650.2.5.17.1
 1.00e+13 ohm-cm1.00e+13 ohm-cmE - 24/125; IPC-TM-650.2.5.17.1
Surface Resistance 1.00e+12 ohm1.00e+12 ohmC - 96/35/90; IPC-TM-650.2.5.17.1
 1.00e+12 ohm1.00e+12 ohmE - 24/125; IPC-TM-650.2.5.17.1
Dielectric Constant  3.8
@Frequency 1e+10 Hz
3.8
@Frequency 1e+10 Hz
Split Post Cavity; Internal Method
 4.0
@Frequency 1e+9 Hz
4.0
@Frequency 1e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Dielectric Strength 39.4 kV/mm1000 kV/inIPC-TM-650.2.5.6.2
Dielectric Breakdown >= 50000 V>= 50000 VIPC-TM-650.2.5.6
Dissipation Factor  0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
 0.016
@Frequency 1e+10 Hz
0.016
@Frequency 1e+10 Hz
Split Post Cavity; Internal Method
Arc Resistance 158 sec158 secIPC-TM-650.2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.0 - 17.0 µm/m-°C
@Temperature -40.0 - 125 °C
6.67 - 9.44 µin/in-°F
@Temperature -40.0 - 257 °F
X/Y; IPC-TM-650.2.4.41
 65.0 µm/m-°C
@Temperature 50.0 - 165 °C
36.1 µin/in-°F
@Temperature 122 - 329 °F
Z-Axis Alpha 1; IPC-TM-650.2.4.41
 250 µm/m-°C
@Temperature 165 - 260 °C
139 µin/in-°F
@Temperature 329 - 500 °F
Z-Axis Alpha 2; IPC-TM-650.2.4.41
Specific Heat Capacity 0.962 J/g-°C0.230 BTU/lb-°FASTM E1461-92
Thermal Conductivity 0.470 W/m-K3.26 BTU-in/hr-ft²-°FASTM E1461-92
Glass Transition Temp, Tg 155 °C311 °FTMA; IPC-TM-650.2.4.24c
 165 °C329 °FDSC; IPC-TM-650.2.4.25c
 190 °C374 °FDMA; IPC-TM-650.2.4.24.3
Decomposition Temperature 425 °C797 °F5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0V-0
 
Descriptive Properties
Methylene Chloride Resistance (% Weight Change)0.02IPC-TM-650.2.3.4.3
Pressure CookerPass60 min then solder dip @288ºC until failure (max 10 min.); IPC-TM-650.2.6.16 (modified)
T260 (minutes)>30IPC-TM-650.2.4.24.1
T288 (minutes)2-4IPC-TM-650.2.4.24.1
Z Axis Expansion (%)3.550ºC to 260ºC; IPC-TM-650.2.4.41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
Park Aerospace Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg
Park Aerospace Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg
Park Aerospace Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg
Park Aerospace Nelco® N4380-13 RF Microwave Performance, Modified Epoxy

PPARK114 / 89386

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.