MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics PEEK Film Made from VICTREX™ Polymer
Categories: Polymer; Film; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Extremely high temperature resistance and continuous use temperature. Excellent flexural and tensile properties. Good abrasion and rain erosion resistance. Excellent chemical resistance. Excellent electrical properties.

Information provided by Westlake Plastics.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.256 g/ccASTM D792
Water Absorption 0.40 %ASTM D570; 24 hrs.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17400 psiASTM D882
Elongation at Break 50 %ASTM D882
Tensile Modulus 391500 psiASTM D882
Flexural Modulus 531000 psiASTM D790
Tear Strength 14.0 kg(f)/cmASTM D1004
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.80e+15 ohmASTM D257
Dielectric Constant 3.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 3200 V/mil
@Thickness 0.0762 mm
ASTM D149
Dissipation Factor 0.0026
@Frequency 10000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 644 °FDSC
Maximum Service Temperature, Air 464 °FContinuous Use
Deflection Temperature at 1.8 MPa (264 psi) 330 °FASTM D648
Glass Transition Temp, Tg 142.7 °CASTM D3418
Flammability, UL94 V-0VTM-1
Smoke Density <= 1.0NBS; ASTM E662
Oxygen Index 23 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
Mitsubishi Chemical Advanced Materials Ketron™ CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
VICTREX™ PEEK 450G903 Black Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron™ LSG PEEK Extruded Unfilled Polyetherether Ketone
VICTREX™ PEEK 150CA30 30% Carbon Fiber Reinforced

PWEST080 / 72739

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.