MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson DTDM-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% morpholine disulfide (4,4'-dithiodimorpholine), 20% EPDM/EVA binder and dispersing agents

Use Characteristics: The curing accelerator Konson® DTDM-80 liberates free sulphur which, in contrast to normal sulphur, mainly forms mono and diether bridges under normal curing conditions. These are responsible for excellent heat ageing resistance of the vulcanizates. Konson® DTDM-80 causes no blooming effects which are generally observed when using thiuramdisulphides as crosslinking agents. In contrast to compounds with Konson®CLD-80, compounds with Konson® DTDM-80 stand out for their increased safety in scorch properties. When the full curing temperature is reached, a quick vulcanization follows. Acid compounding ingredients may cause a premature decomposition of Konson® DTDM-80 and thus reduce the excellent scorch safety (long scorch time). In general the use of Konson® DTDM-80 is recommended whenever favourable compression set behaviour and advantageous ageing behaviour is required.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective DTDM is assured.

Applications: articles resistant to reversion based on NR, such as tyre carcasses and age-resistant articles based on SBR, NBR and EPDM.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.22 g/cc0.0368 - 0.0441 lb/in³
Ash <= 0.50 %<= 0.50 %
Evaporation Loss <= 0.50 %<= 0.50 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 118 °C244 °F
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 25 - 29 %25 - 29 %
 
Descriptive Properties
AppearanceGrey granules
Content= 96 %DTDM
Sieve residue= 0.8 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS029 / 256074

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.