MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rogers Arlon DiClad 870 PTFE/Woven Fiberglass Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Extremely Low Loss Tangent
  • Excellent Dimensional Stability
  • Product Performance Uniformity

Benefits:

  • Electrical Properties are highly uniform across frequency
  • Consistent Mechanical Performance
  • Excellent Chemical Resistance

Typical Applications:

  • Military Radar Feed Networks
  • Commercial Phased Array Networks
  • Low Loss Base Station Antennas
  • Missile Guidance Systems
  • Digital Radio Antennas
  • Filters, Couplers, LNAs

Information provided by Arlon Materials for Electronics (MED); now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.26 g/cc0.0816 lb/in³ASTM D792 Method A
Water Absorption 0.020 %0.020 %IPC TM-650 2.6.2.2
Outgassing - Total Mass Loss  0.010 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.010 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
Water Vapor Recovered; NASA SP-R-0022A
 0.020 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.020 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
NASA SP-R-0022A
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.00 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
NASA SP-R-0022A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 77.2 MPa11200 psiCross; ASTM D882
 103 MPa14900 psiMachine; ASTM D882
Modulus of Elasticity 2.39 GPa346 ksiCross; ASTM D638
 3.34 GPa485 ksiMachine; ASTM D638
Flexural Modulus >= 3.01 GPa>= 437 ksiASTM D790
Compressive Modulus 2.25 GPa327 ksiASTM D695
Peel Strength 2.45 kN/m14.0 pliAfter Thermal Stress; IPC TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+15 ohm-cm1.50e+15 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 3.40e+13 ohm3.40e+13 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant  2.33
@Frequency 1e+6 Hz
2.33
@Frequency 1e+6 Hz
C23/50; IPC TM-650 2.5.5.3
 2.33
@Frequency 1e+10 Hz
2.33
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Dielectric Breakdown >= 45000 V>= 45000 VD48/50; ASTM D149
Dissipation Factor  0.00090
@Frequency 1e+6 Hz
0.00090
@Frequency 1e+6 Hz
C23/50; IPC TM-650 2.5.5.3
 0.0013
@Frequency 1e+10 Hz
0.0013
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Arc Resistance >= 180 sec>= 180 secD48/50; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 0.000 - 100 °C
9.44 µin/in-°F
@Temperature 32.0 - 212 °F
x direction; IPC TM-650 2.4.24
 29.0 µm/m-°C
@Temperature 0.000 - 100 °C
16.1 µin/in-°F
@Temperature 32.0 - 212 °F
y direction; IPC TM-650 2.4.24
CTE, linear, Transverse to Flow 217 µm/m-°C
@Temperature 0.000 - 100 °C
121 µin/in-°F
@Temperature 32.0 - 212 °F
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.257 W/m-K
@Temperature 100 °C
1.78 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1225
Flammability, UL94 V-0V-0Vertical Burn
 
Descriptive Properties
Temperature Coefficient of Dielectric (ppm/°C)-161IPC TM-650 2.5.5.5 (-10 - 140°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced
Rogers Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates
Chevron Phillips Marlex® HGX-030-02 Polypropylene Fiber Resin
Rogers Arlon DiClad 880 PTFE/Woven Fiberglass Laminate
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled

PARLM9890 / 149043

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.