MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TechnoCompound TechnoPet GF 20 2 0 PET, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: The TechnoPet compound line contains non-reinforced, glass fiber reinforced, impact strength modified as well as UV stabilized compounds for outdoor use. TechnoPet compounds offer these properties:
High stiffness
High thermal stability > 220 °C
Attractive surface
High dimensional stability
For these reasons they represent an extremely cost effective solution compared with other technical compounds.

Typical Applications:

  • Automotive industry: e.g. as a substitute for PA, engine covers
  • Electrical engineering: e.g. lamp holders: glass fiber reinforced, flame retardant, high stiffness; multiple power sockets: modified impact strength, high dimensional accuracy
  • Household appliances: e.g. steam irons: thermally stabilized PET compound
  • Packaging/logistics: e.g. logistic systems: modified impact strength, structural stability and strength
  • Mechanical engineering: castors, bearings, gears, guide slide bearings

Information provided by TechnoCompound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccISO 1183
Water Absorption 0.20 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 0.45 %Humidity; ISO 62
Viscosity Number 66 cm³/gISO 1628-5
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Pressure 60.0 MPa,
Temperature 275 °C
WZ 135 bzw. 100°C; ISO 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
@Pressure 60.0 MPa,
Temperature 275 °C
WZ 135 bzw. 100°C; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 230 MPa
@Load 36.5 kg
ISO 2039-1
Tensile Strength at Break 130 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ISO 527
Tensile Modulus 8000 MPa1 mm/min; ISO 527
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
 25.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60093
Dielectric Constant 4.1
@Frequency 1e+6 Hz
IEC 60251
 4.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength 31.0 kV/mm
@Thickness 1.00 mm
Short Time; IEC 60243-1
Comparative Tracking Index 250 VA; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
Melting Point 240 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75
Deflection Temperature at 8.0 MPa 75.0 °CISO 75
Vicat Softening Point 250 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
Glow Wire Flammability Index 750 °CIEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTECHNO052 / 306414

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.