MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ganpati Exim 930dtex/1 (840D/1) Nylon-6 dipped tire cord
Categories: Other Engineering Material

Material Notes: The Nylon-6 dipped tire cord is a high and new technology product. It has such advantages as follows:
  • High breaking strength
  • Excellent impact resistance
  • High fatigue-proof strength
  • Good adhesive strength with rubber
  • Its is the high quality framework material of all kinds of rubber tire.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 65.0 MPaQualified product
 >= 67.0 MPaFirst quality
 >= 69.0 MPaBest quality
Elongation at Break 6.7 - 8.3 %
@Load 2.29 kg
Best quality
 6.5 - 8.5 %
@Load 2.29 kg
First quality
 6.5 - 8.5 %
@Load 2.29 kg
Qualified product
 
Thermal PropertiesOriginal ValueComments
Shrinkage <= 4.0 %
@Temperature 150 °C,
Time 1800 sec
Best quality, in Hot Air
 <= 4.0 %
@Temperature 150 °C,
Time 1800 sec
First quality, in Hot Air
 <= 4.0 %
@Temperature 150 °C,
Time 1800 sec
Qualified product, in Hot Air
 
Descriptive Properties
Adhesion by H-Test>44 N/cmQualified product
 >49 N/cmFirst quality
 >54 N/cmBest quality
Cord Gauge0.29-0.35 mmBest quality
 0.29-0.35 mmFirst quality
 0.29-0.35 mmQualified product
Resin Pick up3.0-5.4%First quality
 3.0-5.4%Qualified product
 3.2-5.2%Best quality
Variation of Elongation<6.0%Best quality
 <6.5%First quality
 <7.0%Qualified product
Variation of Tensile<4.0%Best quality
 <4.5%First quality
 <5.0%Qualified product
Water Ratio<1.0%Best quality
 <1.0%First quality
 <1.0%Qualified product
Z-Twist19.5-22.5 T/10cmBest quality
 19.5-22.5 T/10cmFirst quality
 19.5-22.5 T/10cmQualified product

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI019 / 317303

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.