MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Apcotex Apcoflex® NVC70E NBR/PVC Rubber Polyblend
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Apcoflex® NVC70E* is a blend of Apcoflex medium NBR and PVC in 70:30 ratio. .It contains non-staining stabilizer and comes in light tan colored sheet form.

Applications: Apcoflex® NVC70E is a Polyblend of Nitrile Rubber with PVC; hence, it provides Oil, Fuel, Thermal resistance as well as Ozone and environmental resistance. . It is recommended for the manufacture of extruded and molded products suitable for out-door applications in automotive and industrial applications. . This is cost effective medium ACN blend for general purpose automotive and industrial molded and extruded products.

CAS No: 9003-18-3 : NBR/ 9002-86-2 : PVC

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.70 %
Mooney Viscosity 45 - 55
@Temperature 100 °C
ML 1+4
Ash <= 1.0 %
Storage Temperature <= 35.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life <= 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPCOT013 / 315592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.