MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ITW Devcon® Permatex® Zip Grip® GPE 15 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: A single component low viscosity, fast setting, cyanoacrylate adhesive. Ideal for fast setting bonds for rubber bonding applications. Features: Easy to apply, Fixtures in seconds, Permanent, Enhanced toughness to peel and shock loads, Highly resistant to aging and weathering,Rubber Bonder.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccUncured
Viscosity 15 cP15 cP
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 22.1 MPa3200 psiAdhesive Tensile Shear; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.30e+14 ohm-cm5.30e+14 ohm-cm
Dielectric Constant 5.4
@Frequency 1000 Hz
5.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 11.6 kV/mm295 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 227 µm/m-°C126 µin/in-°FASTM D696
Melting Point 165 °C329 °FCured 7 days @ 75° F
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point 85.0 °C185 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49cured
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0667 - 0.167 min0.00111 - 0.00278 hourPlastic
 0.0833 - 0.167 min0.00139 - 0.00278 hourSteel
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
As Tested
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Chemical TypeEthyl cyanoacrylate
Chemical/Solvent Resistance1,1,1-Trichloroethane: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Motor Oil: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: poor30 day immersion at 75°F. Sample cured 7 days at RT
Colorcolorlessliquid. Uncured
Gap Filling (in)0.005Uncured
Military SpecificationMil-A-46050C Type II, Class 2
SolubilityNitromethane, AcetoneCured.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWP9167 / 239677

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.