MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Powersil® 351 MH Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 351 MH is a peroxide curing silicone elastomer with excellent electrical and mechanical properties especially suitable for outdoor applications in the T&D-sector.

Special features:

  • ready to use, one component system
  • excellent elongation at break, high tear strength
  • very good dielectrical properties
  • good tracking resistance
  • very good arc resistance
Application: POWERSIL® 351 MH is especially designed for T<(>&<)>D applications. Because of its excellent mechanical properties POWERSIL® 351 MH is prone for use in “cable accessories” applications.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccDIN 51757
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38ISO 868
Tensile Strength at Break 9.00 MPaISO 37
Elongation at Break 800 %ISO 37
Tear Strength 30.0 kN/mASTM 624 B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.8
@Frequency 50 Hz
IEC 60250
Dielectric Strength 23.0 kV/mm
@Thickness 1.00 mm
IEC 60243
Dissipation Factor 0.00020
@Frequency 50 Hz
IEC 60250
Arc Resistance >= 240 secIEC 61621
 
Descriptive Properties
Colorgray
Track Resistance1A 3.5IEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9362 / 204891

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.