MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Silvaloy® 505 Carbide Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 505 readily wets nickel and iron base alloys. It is recommended for joining 300 Series stainless steel and will retard interface corrosion in most exposures for which the base metals are suitable. However, for joints on cupro-nickel exposed to salt water at elevated temperatures, zinc-free alloys such as Braze 559, 603, or 630 should be used to avoid joint failure by dezincification.

Because this alloy is cadmium-free, it can be safely used on food handling equipment and hospital utensils.

The presence of nickel in Braze 505 aids in the joining of small tungsten carbide inserts in cutting tools. In addition, it offsets joint interface brittleness caused by diffusion of aluminum into the brazing alloy, when joining aluminum-bronze to steel.

Characteristics:Braze 505 is very fluid at its flow point and will quickly fill long, narrow joints. Because it has the tendency to liquate (i.e., separate into low and high melting constituents) when heated slowly, this alloy should be heated quickly through its melting range.

Specifications:This filler metal conforms to the following specification-AWS A5.8 BAg-24, SAE AMS 4788

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 66000 - 73300 psi1029 Cold Rolled Steel butt joint.
 69500 - 88000 psi18-8 Annealed Stainless Steel butt joint.
Elongation at Break 1.0 - 9.0 %% in 2", 18-8 Annealed Stainless Steel butt joint
 15 - 25 %% in 2", 1029 Cold Rolled Steel butt joint.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00001195 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1220 - 1305 °F
Solidus 1220 °FMelting Point
Liquidus 1305 °FFlow Point
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 19 - 21 %
Nickel, Ni 1.5 - 2.5 %
Other, total <= 0.15 %
Silver, Ag 49 - 51 %
Zinc, Zn 26 - 30 %
 
Descriptive Properties
ColorYellow White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum C443.0-F Die Casting Alloy
H.C. Starck Amperit® 525.2 Sintered Tungsten Carbide - Cobalt (WC-Co) 83-17
Mi-Tech Metals CW75 75 Tungsten/25 Copper PM Metal Composite
304 Stainless Steel
Lucas-Milhaupt Silvaloy® 495 Carbide Brazing Alloy

NLUCMI08 / 18075

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.