MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Master Bond UV23FLDC-80TK One component, Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Cures in shadowed out areas with heat
  • Curing temperature 80-85°C
  • Excellent elongation
  • Outstanding thermal cycling properties
Product Description: Master Bond UV23FLDC-80TK is a moderate viscosity, dual curing, cationic type system. It has an initial cure utilizing UV light along with secondary curing in shadowed out areas by heating, typically 60-90 minutes at 80-85°C. The heat curing cycle is most often used to complete the cure, but at times can even be used to initiate fixturing. UV23FLDC-80TK cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections up to 0.25 inches deep and can be used for encapsulation. However, when bonding, sections of a few thousandths of an inch are more than adequate. It does not contain any solvents or diluents, has very low shrinkage upon curing, and is not oxygen inhibited. UV23FLDC-80TK bonds well to a wide variety of substrates including metals, glass, and plastics, particularly acrylics, polycarbonates and other optically clear polymers. It has a service temperature range of -80°F to +300°F. It is a superior electrical insulator and is resistant to water, oils, fuels and mild acids and bases. Most noteworthy is its toughness and flexibility allowing it to withstand rigorous thermal cycling. Some applications for this innovative system would be in fiber optics including mounting optics, bonding fiber terminations into ferrules, laminating and sealing glass plates, especially when low stress upon substrates is an important consideration. It also can be used in electronics as an encapsulant and in semiconductor applications as a glob top.

Product Advantages:

  • Dual cure capability; UV, heat, or both
  • Highly reliable thermal and electrical insulator
  • Can withstand thermal cycling and shock
  • Low modulus, low stress
  • High elongation

Information provided by Master Bond, Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/cc
Viscosity 25000 - 50000 cP25000 - 50000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45.0 - 55.045.0 - 55.0
Tensile Strength 0.689 - 1.38 MPa100 - 200 psi
Elongation at Break 90.0 - 100 %90.0 - 100 %
Tensile Modulus 0.00172 - 0.00345 GPa0.250 - 0.500 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.70
@Frequency 60 Hz
4.70
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 80.0 µm/m-°C38.9 - 44.4 µin/in-°F
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -62.0 °C-79.6 °F
Glass Transition Temp, Tg 35.0 - 45.0 °C95.0 - 113 °Fwith post cure
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
in original, unopened containers
 
Descriptive Properties
Thixotropic index5.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5813 / 323330

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.