MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:

Information provided by Ravago.

Key Words: High Flow
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Water Absorption 0.14 %0.14 %24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Melt Flow 22 - 28 g/10 min
@Load 3.80 kg,
Temperature 230 °C
22 - 28 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 79.3 MPa11500 psiASTM D638
Elongation at Break 2.2 %2.2 %ASTM D638
Flexural Strength 114 MPa16500 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 4.00e+16 ohm-cm4.00e+16 ohm-cmASTM D257
Dielectric Strength 16.1 kV/mm
@Thickness 3.17 mm
410 kV/in
@Thickness 0.125 in
in Air; ASTM D149
Arc Resistance 120 sec120 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °FASTM D648
Vicat Softening Point 149 °C300 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 - 271 °C490 - 520 °F
Middle Barrel Temperature 266 - 277 °C510 - 530 °F
Front Barrel Temperature 271 - 282 °C520 - 540 °F
Nozzle Temperature 271 - 288 °C520 - 550 °F
Melt Temperature 271 - 293 °C520 - 560 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hour
 6 - 8 hour6 - 8 hourwith regrind
Injection Pressure 5.52 - 11.0 MPa800 - 1600 psi
Hold Pressure 5.52 - 8.27 MPa800 - 1200 psi
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 40 - 60 %40 - 60 %To Cylinder
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized
Entec Hylex® P1010FR Polycarbonate
Entec Hylex® P1010L1 HB Polycarbonate
Ravago Manufacturing Americas Hylex® P1010G20 HB Polycarbonate, 20% Fiberglass Reinforced
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced

PENTA049 / 36072

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.