MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro MAKROFOL® UV 244 6-2 040004 Polycarbonate Films
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Makrofol UV 244 6-2 040004 is an coextruded film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol UV 244 6-2 040004 is an coextruded film with a specially developed functional layer for UV protection. It combines the well known advantages of Makrofol with respect to mechanical, thermal and optical properties, with the capability for applications under UV exposure. Typical applications are instrument panels and touch panels in the automotive sector. Makrofol UV 244 6-2 040004 is available in standard thicknesses of 0.010" and 0.015" (250 microns and 375 microns). Other thicknesses are available on request. The surface structure of Makrofol UV 244 6-2 040004 is one side fine velvet and one side very fine matte. As with any product, use of Makrofol UV 244 6-2 040004 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccISO 1183, Method C
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 60.0 MPa>= 8700 psiISO 527-1,-3
Elongation at Break >= 100 %>= 100 %ISO 527-1,-3
Tensile Modulus >= 2.10 GPa>= 305 ksiISO 527-1,-3
 
Optical PropertiesMetricEnglishComments
Gloss 2.0 - 8.0 %2.0 - 8.0 %60°, 6-surface; ISO 2813
 <= 90 %<= 90 %60°, 2- surface; ISO 2813
Transmission, Visible >= 80 %>= 80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro MAKROFOL® HF312 G-4 020021 Polycarbonate Films
Covestro Makrofol® DE 7-2 Polycarbonate
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® ID 6-2 laserable Polycarbonate
Covestro Makrofol® ID 4-4 white Polycarbonate

PCOVEST0815 / 202598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.