System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Almaak Anjaflam® PC/ABS 050/85S-FR PC/ABS, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
Material Notes:
unreinforced, easy flowing, flame retarded (V-0), natural color
Information provided by Almaak International GmbH.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.19
g/cc
0.0430
lb/in³
ISO 1183
Water Absorption
0.70 %
0.70 %
ISO 62
Moisture Absorption
0.200 %
0.200 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ISO 294-4
Melt Flow
26
g/10 min
@Load 5.00 kg,
Temperature 260 °C
26
g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
60.0
MPa
8700
psi
50 mm/min; ISO 527-1/2
Elongation at Break
4.0 %
4.0 %
50 mm/min; ISO 527-1/2
Modulus of Elasticity
2.50
GPa
363
ksi
1 mm/min; ISO 527-1/2
Charpy Impact Unnotched
NB
NB
ISO 179/1eU
Charpy Impact, Notched
4.00
J/cm²
19.0
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Dielectric Strength
30.0
kV/mm
762
kV/in
IEC 60243
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
100
°C
212
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
90.0
°C
194
°F
ISO 75
Vicat Softening Point
110
°C
@Load 5.10 kg
230
°F
@Load 11.2 lb
50K/h; ISO 306
Flammability, UL94
V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Flammability Index
960
°C
@Thickness 4.00 mm
1760
°F
@Thickness 0.157 in
DIN EN 60695-2-12
Processing Properties
Metric
English
Comments
Melt Temperature
240
-
280
°C
464
-
536
°F
Mold Temperature
60.0
-
80.0
°C
140
-
176
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
4.00
-
6.00
hour
4.00
-
6.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Descriptive Properties
Quality level
Virgin
DIN EN ISO 14021
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLMA9926 / 316554
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.