MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F652 Bismaleimide Resin
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: HexPly® F652 is a bismaleimide resin that cures via an addition reaction with no condensation by-products. HexPly® F652 is a controlled flow polyimide resin system designed for alternative processing capabilities such as co-curing over honeycomb core, compression molding, as well as standard autoclave processing.

Information provided by HexCel

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/cc
Moisture Absorption at Equilibrium 4.4 %
 
Mechanical PropertiesOriginal ValueComments
Fracture Toughness 0.639 MPa-m½
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.01
@Frequency 1.60e+10 Hz,
Temperature 24.0 °C
+/- 2%; ASTM D2520
 3.05
@Frequency 9.00e+9 Hz,
Temperature 24.0 °C
+/- 2%; ASTM D2520
 3.05
@Frequency 1.60e+10 Hz,
Temperature 149 °C
+/- 2%; ASTM D2520
 3.08
@Frequency 9.00e+9 Hz,
Temperature 149 °C
+/- 2%; ASTM D2520
 3.09
@Frequency 3.00e+9 Hz,
Temperature 24.0 °C
+/- 2%; ASTM D2520
 3.09
@Frequency 1.60e+10 Hz,
Temperature 232 °C
+/- 2%; ASTM D2520
 3.12
@Frequency 9.00e+9 Hz,
Temperature 232 °C
+/- 2%; ASTM D2520
 3.13
@Frequency 3.00e+9 Hz,
Temperature 149 °C
+/- 2%; ASTM D2520
 3.17
@Frequency 3.00e+9 Hz,
Temperature 232 °C
+/- 2%; ASTM D2520
Dielectric Loss Index 0.0050
@Frequency 3.00e+9 Hz,
Temperature 24.0 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0060
@Frequency 3.00e+9 Hz,
Temperature 149 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0060
@Frequency 9.00e+9 Hz,
Temperature 24.0 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0070
@Frequency 3.00e+9 Hz,
Temperature 232 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0070
@Frequency 9.00e+9 Hz,
Temperature 149 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0070
@Frequency 1.60e+10 Hz,
Temperature 24.0 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0080
@Frequency 9.00e+9 Hz,
Temperature 232 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0080
@Frequency 1.60e+10 Hz,
Temperature 149 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 0.0090
@Frequency 1.60e+10 Hz,
Temperature 232 °C
F652 Resin Casting; +/- 0.5; ASTM D2520
 
Thermal PropertiesOriginal ValueComments
CTE, linear 52.0 µm/m-°C
@Temperature 24.0 - 299 °C
Glass Transition Temp, Tg >= 232 °CWet
 >= 316 °CDry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® F650 Bismaleimide Resin
Hexcel® HexPly® F655 Bismaleimide Resin
Hexcel® HexPly® M65 Bismaleimide Resin
Solvay HTM® 552 Bismaleimide Resin
Solvay CYCOM® 5250-4 BMI Prepreg Neat Resin

PHEXC008 / 98478

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.