Moplen BA238A is a non-filled copolymer for injection molding with very high impact strength. This grade is natural, in pellet form. Typical applications for Moplen BA238A are painted bumpers. Product Features: Painted Bumpers/ High impact resistance required application Typical Applications: high impact strength even at low temperature Information provided by PolyMirae |