MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 6300HG ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: ALLEN® 6300HG is a high gloss acrylic capped ABS with excellent outdoor weathering and durability.

ALLEN® 6300HG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Lawn and Garden Equipment
  • Marine Parts
  • Heavy Equipment Exteriors
  • Recreational Vehicles
  • Kayaks
Features:
  • Custom color matching
  • UV protection
  • Good abrasion resistance
  • Low gloss finish
  • Excellent color and gloss retention
  • Good chemical resistance

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Water Absorption 0.340 %0.340 %equilibrium; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 99.099.0ASTM D785
Tensile Strength 41.0 MPa5950 psiASTM D638
Tensile Modulus 1.979 GPa287.0 ksiASTM D638
Flexural Strength 64.7 MPa
@Strain 5.00 %
9380 psi
@Strain 5.00 %
ASTM D790
Flexural Modulus 1.99 GPa289 ksiASTM D790
Compressive Yield Strength 49.7 MPa7210 psiASTM D695
Bearing Yield Strength <= 182.7 MPa<= 26500 psiASTM D953
 20.9 MPa
@Strain 4.00 %
3030 psi
@Strain 4.00 %
ASTM D953
Shear Strength 37.2 MPa5400 psiASTM D732
Izod Impact, Notched 2.019 J/cm3.782 ft-lb/inASTM D256
Gardner Impact 24.1 J17.8 ft-lbDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 19.6 kV/mm498 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 97.5 µm/m-°C54.2 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C195 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °Fannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0598 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS530 / 325270

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.