MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Solaris® Clear Encapsulant Silicone Encapsulating Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Solaris® is a low viscosity, clear and colorless liquid platinum cure silicone rubber compound designed for use in protecting of electronic components and other assemblies. It will protect components against shock, vibration, moisture, ozone, dust, chemicals and other environmental hazards. The optical clarity of Solaris® makes it suitable for potting solar cells for maximum light transmission or electronic assemblies where component identification is necessary. For best results, use with Solaris® Bonding Primer®.
  • Ultra-transparent Solaris® provides excellent UV resistance yet allows maximum transmission of light.
  • Solaris® features a low viscosity which allows easy flow in and around complex shapes, providing excellent electrical insulation and shock resistance.
  • Solaris® will cure in deep sections or enclosed assemblies without exotherm.
  • Solaris® encapsulant contains no solvents and has no VOC’s.
  • The hydrolytic stability of Solaris® makes it suitable in high humidity environments and at elevated temperatures.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D-1475
Viscosity 1200 cP1200 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1515ASTM D-2240
Tensile Strength 1.24 MPa180 psiASTM D-412
Elongation at Break 290 %290 %ASTM D-412
100% Modulus 0.172 MPa25.0 psiASTM D-412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.16e+15 ohm-cm3.16e+15 ohm-cmASTM D-257
Dielectric Constant 2.78
@Frequency 100 Hz
2.78
@Frequency 100 Hz
ASTM D-150
Dielectric Strength 14.4 kV/mm366 kV/inASTM D-150
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°FASTM D-1461
Maximum Service Temperature, Air 205 °C401 °F
Minimum Service Temperature, Air -100 °C-148 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.411.41ASTM D-1218
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
Pot Life 240 min240 minASTM D-2471
 
Descriptive Properties
ColorClear
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume28.1[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN158 / 296859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.