MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Dow™ DMDB-1210 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDB-1210 NT 7 HDPE is intended for use in intended for use in both compression and injection molded closure applications. This resin has been designed to meet demanding performance requirements, especially in the areas of stiffness, impact strength and sensory, while maintaining good processing characteristics beneficial to molders. Typical applications include injection molded closures for water bottles, where minimizing the contribution of the package to the taste of the product is a requirement.
Main Characteristics:
  • Excellent Stiffness and Impact Strength
  • Excellent Organoleptic Properties
  • Excellent Processing Characteristics
Complies with: US FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; EU No 10/2011. Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; EU No 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D792
ESCR 100% Igepal® 12 hour
@Temperature 50.0 °C
12 hour
@Temperature 122 °F
F50; ASTM D1693
ESCR 10% Igepal® 12 hour
@Temperature 50.0 °C
12 hour
@Temperature 122 °F
F50, Molded and tested in accordance with ASTM D4976; ASTM D1693
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ASTM D2240
Tensile Strength at Break 20.5 MPa2970 psiASTM D638
Tensile Strength, Yield 27.3 MPa3960 psiASTM D638
Elongation at Break 1500 %1500 %ASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus 1.05 GPa152 ksi2% Secant; ASTM D790B
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °F
Vicat Softening Point 125 °C257 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF457 / 311150

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.