MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Materion Ytterbium Fluoride, YbF3
Categories: Ceramic; Halide

Material Notes: Ytterbium Fluoride, YbF3, is a low-index film material that exhibits good transparency from the UV through far-infrared regions. The films are insoluble and show low stress, making YbF3 a useful substitute for ThF4 in many IR applications. It can be combined in multi-layers with higher-index ZnS, ZnSe and Ge layers and with other fluoride compounds. Typical applications are in AR, long-wave pass, short-wave pass, and filter coatings in the 3 to 11µm wavelength range. A particular advantage that Ytterbium fluoride coatings provide is the minimum appearance of water absorption bands in the Mid-IR region.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.17 g/cc0.295 lb/in³Crystal
Molecular Weight 230 g/mol230 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1157 °C2115 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.529
@Wavelength 2250 nm
1.529
@Wavelength 2250 nm
 1.532
@Wavelength 1050 nm
1.532
@Wavelength 1050 nm
 1.536
@Wavelength 650 nm
1.536
@Wavelength 650 nm
 1.537
@Wavelength 450 nm
1.537
@Wavelength 450 nm
 1.54
@Wavelength 400 nm
1.54
@Wavelength 400 nm
 1.545
@Wavelength 350 nm
1.545
@Wavelength 350 nm
 1.557
@Wavelength 300 nm
1.557
@Wavelength 300 nm
 1.57
@Wavelength 275 nm
1.57
@Wavelength 275 nm
 
Descriptive Properties
ColorWhite
Evaporation Temperature900°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMATER914 / 323620

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.