MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Pearlbond™ 960 EXP Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: PEARLBOND™ 960 EXP is an aliphatic plasticizer- free polyether-based thermoplastic polyurethane. It combines excellent mechanical properties with excellent low temperature flexibility.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccISO 2781
Melt Flow 1.0 - 12 g/10 min
@Load 2.16 kg,
Temperature 177 °C
1.0 - 12 g/10 min
@Load 4.76 lb,
Temperature 351 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  60
@Time 86400 sec
60
@Time 24.0 hour
ISO 868
 69
@Time 1.81e+6 sec
69
@Time 504 hour
ISO 868
Tensile Strength 44.0 MPa6380 psiISO 527
Elongation, Ultimate 510 %510 %ISO 527
100% Modulus 2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
ISO 527
300% Modulus 7.00 MPa
@Strain 300 %
1020 psi
@Strain 300 %
ISO 527
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 - 180 °C338 - 356 °FMQSA 70A
Softening Point 125 - 135 °C257 - 275 °FMQSA 70A
 
Processing PropertiesMetricEnglishComments
Zone 1 140 - 150 °C284 - 302 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 185 - 200 °C365 - 392 °F
Zone 4 185 - 200 °C365 - 392 °F
Die Temperature 180 - 190 °C356 - 374 °F
Drying Temperature 60.0 - 70.0 °C
@Time 14400 - 18000 sec
140 - 158 °F
@Time 4.00 - 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5044 / 238914

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.