MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® LDPE PCG06 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE grades for healthcare applications are produced under controlled conditions resulting in high product quality, consistency and a high level of purity. SABIC® LDPE PCG06 is an additive-free grade with high purity and very low migration levels. It is typically used for semi-rigid IV containers for Large Volume Parenterals (LVP) obtained by Blow Fill Seal (BFS) process. Compliance to Regulations SABIC® LDPE PCG06 complies with the relevant monographs of the European Pharmacopoeia (EP) and the United States Pharmacopoeia (USPVI).

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 0.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psiISO 527-3
Film Tensile Strength at Yield, TD 14.0 MPa2030 psiISO 527-3
Film Elongation at Break, MD >= 200 %>= 200 %ISO 527-3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-3
Tensile Modulus 0.290 GPa42.1 ksiMD; ISO 527-3
 0.340 GPa49.3 ksiTD; ISO 527-3
Coefficient of Friction 1.01.0ASTM D1894
Tear Strength 35.0 kN/m200 pliTD; ISO 6383-2
 45.0 kN/m257 pliMD; ISO 6383-2
Dart Drop Total Energy 250 J/cm0.468 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 21.0 MPa3050 psiISO 527-3
Film Tensile Strength at Break, TD 22.0 MPa3190 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 115 °C239 °FDIN 53765
Vicat Softening Point 106 °C223 °Fat 10 N (VST/A); ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %6.0 %ASTM D1003
Gloss 70 %70 %45°; ASTM D2457
 
Descriptive Properties
Blocking10 gSABIC method
Re-blocking30 gSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11016 / 244483

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.