BETAFORCE™ MP 4000 is a one component, heat curing adhesive with excellent sag and bead stability. The adhesive cures with heat when heated above 100°C. Curing times depend on temperature and application dimension. BETAFORCE™ MP 4000 is a fast heat cure adhesive with good mechanical properties and can be used for microinjection bonding, add-on bonding and composite bonding. DuPont Automotive products are primarily developed in co-operation with the automobile manufacturers, according to their needs and their specifications, they are approved for the specific applications as defined by the customer. Unless specified otherwise test are conducted at 23°C/50% relative humidity.Information provided by DuPont. |