Long carbon fiber reinforced PA6, CF20%, PA6-CF20. General Torayca™ Notes: TORAYCA™ is a carbon fiber reinforced thermoplastic (CFRTP) that is light weight and features excellent strength, stiffness, dimensional accuracy, and sliding properties. Physical property: Carbon fiber reinforced thermoplastic (CFRTP) offer excellent mechanical strength/rigidity and maintain a combination of characteristics. Lower specific gravity and lightweight, High creep resistance and fatigue resistance, Excellent abrasion resistance and sliding properties. Low molding shrinkage and coefficient of linear expansion, ensuring high dimensional accuracy, Excellent electrical conductivity and electromagnetic shielding performance. Information provided by Toray Resin Co. |