MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Wingate Alloys Winco NT 24 Nitrogen-Strengthened Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Winco NT 24 provides good aqueous corrosion resistance combined with resistance to abrasives, metal-to-metal wear and sustained heats of 1500°F. Higher mechanical properties than standard austenitic grades. Outstanding corrosive wear resistance under many different sliding conditions. Galling resistance equivalent to 304 stainless steel.

General Properties: Winco NT 24 has annealed mechanical properties, which are well above those of typical austenitic grades such as 304. This higher strength affords the opportunity to reduce thickness or equivalent engineering loads. Galling resistance of Winco NT 24 is approximately equal to 304. It work hardens rapidly while retaining good ductility. Unlike other nitrogen-strengthened stainless steels, Winco NT 24 is subject to magnetic transformation when cold worked. Winco NT 24 exhibits outstanding corrosive wear resistance under many different sliding conditions. It is more cost effect than 409 and 304 which are typically used in wear abrasive applications.

    Typical Applications:
  • Coal handling equipment-screens, chute liners, buckets and hopper cars.
  • Water supply and control structures.
  • Sewage treatment plant structures.
  • Mining equipment – magnetic ore separator screens.
  • Bulk solids handling equipment – conveyor parts.
  • Mixing tanks.
  • Wear plates, now using less cost-effective materials such as abrasion resistant steels, 409 or 304 stainless steels.
  • Transport and vibratory equipment where fatigue resistance is a major design criteria.
  • Shipboard containers.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.86 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 241<= 241
Hardness, Rockwell B <= 100<= 100
Tensile Strength >= 655 MPa>= 95000 psi
Tensile Strength, Yield >= 331 MPa>= 48000 psi
Elongation at Break >= 35 %>= 35 %2[in]
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 15 - 17 %15 - 17 %
Iron, Fe 69.6 - 76.35 %69.6 - 76.35 %
Manganese, Mn 7.0 - 9.0 %7.0 - 9.0 %
Nickel, Ni 1.5 - 3.0 %1.5 - 3.0 %
Nitrogen, N 0.15 - 0.30 %0.15 - 0.30 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for T 300 Series Stainless Steel
302 Stainless Steel, annealed strip
301 Stainless Steel
430 Stainless Steel annealed at 815°C
ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal

NWINGA13 / 122077

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.