MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 832-5 Flexible Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 832-5 is a flexible two component epoxy which is intended for bonding materials with mis-matched coefficients of expansion. It exhibits flexibility associated with polyurethanes but does not have the moisture sensitivity which usually creates bubbles during the application and cure of urethanes. TRA-BOND 832-5 has been found to be useful in such applications as bonding optical lenses in aluminum housings. As an example two three-inch long glass microscope slides were bonded to opposite sides of a 0.064 inch thick piece of aluminum and the sandwich was cycled from -75°C to 125°C ten times with no spalling of the glass or bond failure.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption 3.0 %100% RH & 85°C
Viscosity 650 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
Adhesive Bond Strength 1000 psiLap shear, alum to alum
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°C
@Temperature -118 - -54.0 °C
 81.0 µm/m-°C
@Temperature -54.0 - -32.0 °C
 173 µm/m-°C
@Temperature -32.0 - 25.0 °C
 224 µm/m-°C
@Temperature 25.0 - 66.0 °C
Glass Transition Temp, Tg -32.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 100 °C
 8.00 hour
@Temperature 75.0 °C
Working Life 8.00 hour
 
Descriptive Properties
Color BlueMixed
Mix Ratio, parts by weight100/143Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Durabond® U-10FL Urethane Adhesive
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Trelleborg Emerson & Cuming Eccobond® G 909 One-Component Fast Cure Epoxy Adhesive
Tra-Con Tra-Bond FS152C Clear Low Viscosity Epoxy Adhesive
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant

PTRAC171 / 71099

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.