MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Devcon Tile Adhesive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Abrasion-Resistant System

Comments: Putty

Data provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0521 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ASTM D2240
Tensile Strength, Ultimate 2640 psiASTM D638
Tensile Modulus 800 ksiASTM D638
Flexural Yield Strength 5480 psiASTM D790
Compressive Yield Strength 8620 psiASTM D695
Adhesive Bond Strength 2890 psiAdhesive tensile shear strength; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 46ASTM D150
Dielectric Strength 320 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.00125 cal cm/sec-cm²-°CASTM C177
Maximum Service Temperature, Air 200 °FOperating Temperature
Shrinkage 0.10 %During Cure; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 °F
Pot Life 120 - 180 min
@Temperature 23.9 °C
 
Descriptive Properties
Coverage per lb.76.4 in²at 1/4 inch thick
Mix Ratio by Volume1 to 1resin:hardener
Mix Ratio by Weight10 to 9resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Bostik Professional Grade™ Ceramic Tile Mastic
Bostik Glass-Mate™ Glass Tile Mortar
Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
Bostik Big Tile & Stone™ Latex-Modified Mortar

PITWX25 / 48512

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.