MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Abatron AboWeld 48-14/AboCure 48-14 Adhesive/Casting Resin
Categories: Polymer; Adhesive; Thermoset

Material Notes: Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend allows for visual inspection of proper mixing and ratios. Shelf life: 12+ months (unmixed).

Processing: 100/(100-150) ratio. Thixotropic (Vaseline-like consistency) Pot life: 100 g, 8-11 hours at 25°C(77°F). Hardens in 2-4 days at 25°C (77°F), 30-40 min. at 80°C (175°F), 20-25 min. at 120°C (250°F), 15-20 min. at 150°C (300°F).

Corrosion Resistance: good resistance to atmospheric conditions, soft and salt water, alkalis and diluted acids.

Key Words: potting, casting, encapsulating, impregnating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %after 24 hrs.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080100/40 pbw; 68 at 100/80 pbw; 66 (60 after 10 sec) at 100/100 pbw
Tensile Strength, Ultimate 51.0 MPa7400 psiTypical averaged test results for Abatron Adhesive/Casting Resins.
Elongation at Break 3.0 %3.0 %Typical for Abatron Adhesive/Casting Resins.
Flexural Yield Strength 83.0 MPa12000 psiTypical averaged test results for Abatron Adhesive/Casting Resins.
Compressive Yield Strength 115 MPa16700 psiTypical averaged test results for Abatron Adhesive/Casting Resins.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboWeld 8101-6/AboCure 8101-6 Epoxy
Kazanorgsintez Polyethyleneglycol-13
Donnelly Bros APG #2 Super Clean All Purpose Mold Grease
CHT Group QGel 300 QSI Quantum Silicones High Strength Gel
CHT Group MM828 Low Tear Condensation Cure 2-Part Molding Rubber

PABKD1 / 22029

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.