MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Duct 8205 One-Part Electrically Conductive Silver-Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 8205 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of excellent mechanical and electrical properties. TRA-DUCT 8205 is a one-part system ideal for high speed manufacturing in the microelectronic, automotive, computer and telecommunications assembly and packaging industries. TRA-DUCT 8205 provides high electrical and thermal conductivity along with excellent adhesion to numerous substrate materials making it excellent for chip/die bonding or heat sink attach. Typical applications include high speed component attachment of electronic modules, printed circuit board assembly and high frequency shielding, when screen printing or automatic dispensing is desired.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 16000 cP16000 cPMixed (cp #52, 5 rpm)
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 9.65 MPa1400 psiLap shear, alum to alum, 1 hr @ 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00030 ohm-cm
@Temperature 150 °C
0.00030 ohm-cm
@Temperature 302 °F
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 88.0 °C190 °FUltimate Tg, cured 1 hr @ 150°C
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 
Descriptive Properties
Color Silver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron 8602-2 A/B Carbon-Filled Electrically Conductive Epoxy Compound
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy
Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive

PTRAC165 / 71093

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.