MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Copolymer Film Grade

Material Notes: Film Properties. Features: Low gel, good barrier properties.

Applications: Merchandising bags, lamination, co-extrusion.

Data provided by the manufacturer.

Key Words: High Density Polyethylene; Polybutene; Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccASTM D792
Moisture Vapor Transmission 0.150 cc-mm/m²-24hr-atmASTM D1434
Water Vapor Transmission 6.00 g/m²/dayASTM D1434
Oxygen Transmission 55.0 cc-mm/m²-24hr-atmor 2200 cc/m²-atm-24 hr per 25 µm film; 38°C; 90% RH Difference
Melt Flow 0.27 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Film Tensile Strength at Yield, MD 21.0 MPaASTM D882
Film Tensile Strength at Yield, TD 23.0 MPaASTM D882
Film Elongation at Break, MD 600 %ASTM D882
Film Elongation at Break, TD 850 %ASTM D882
Secant Modulus, MD 0.590 GPaASTM D882
Secant Modulus, TD 0.680 GPaASTM D882
Coefficient of Friction 0.30ASTM D1894
Elmendorf Tear Strength, MD 1.00 g/micronASTM D1922
Elmendorf Tear Strength, TD 23.0 g/micronASTM D1922
Dart Drop 0.600 g/micronF 50; ASTM D1709/A
Film Tensile Strength at Break, MD 40.0 MPaASTM D882
Film Tensile Strength at Break, TD 38.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 121 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 230 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Covestro Bayblend® T85 XF Polycarbonate + ABS
Covestro Bayblend® T65 XF Polycarbonate + ABS
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
Global F-7000 High Density Polyethylene

PEHN0R / 35540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.