Description: Cordux™ 654 is a disposable backing material which is used for cell stabilization and vacuum clamping of honeycomb during machining operations. It consists of strong kraft paper, coated on one side with a thin film of thermoplastic, modified epoxy resin. The film is dry and non-tacky at temperatures up to 30°C but as a precaution against storage or transit conditions exceeding that temperature, polythene interleaving is incorporated in the roll of film. Features: - Rapid application and removal
- Suitable for either metallic or non-metallic honeycomb
- No time limit on useable life
- Low cost
- Compatible with most epoxy resin structural adhesives
Information provided by Hexcel Corporation. |