MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Cavamax® W8 FOOD gamma-Cyclodextrin
Categories: Other Engineering Material

Material Notes: Chemical name: gamma-Cyclodextrin, cyclooctaamylose, cyclomaltooctaose CAVAMAX® W8 Food is a food grade gammacyclodextrin. CAVAMAX® W8 Food with 8 glucose units has the largest cavity of the parent cyclodextrins and is the most water soluble. It is useful for solubilizing, stabilizing or delivering larger molecules; e.g. oils, lipids, etc.

Empirical formula: C48H80O40 CAS No.: 17465-86-0

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 - 0.700 g/cc0.0145 - 0.0253 lb/in³
Ash <= 0.1 %<= 0.1 %sulfate ash
Evaporation Loss <= 11 %<= 11 %
 
Descriptive Properties
Appearancesolid powder
Colorwhite
Content<0.5%Reducing substances (determined as dextrose)
 <1 ppmArsenic
 <1 ppmLead
 <1000/gMicroorganisms
 <20 ppmVolatile organic compounds
 <4 ppmHeavy metals
 <4 ppmResidual complexant (8-cyclohexdecan-1-one (CHDC))
 <6 ppmResidual solvent (n-decan)
 >98%Content (on dry basis)
 0 in 10 gSalmonella/E Coli
Solubility180.1 g/lOECD 105, in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9056 / 204585

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.